banner
laser crystal
optical crystal
Energy Level Transition
|
4I3/2→4I11/2
|
Laser Wavelength
|
2940 nm
|
Photon Energy
|
6.75×10-20 J @ 2.940 μm
|
Emission Cross-Section
|
3×10-20 cm2
|
Refractive Index
|
1.79 @ 2.940 μm
|
Pump Band
|
600~800 nm
|
Doping Concentration
|
Er: ~50 at.%
|
Rod Size
|
Diameter: 3~6 mm, Length: 50~120 mm;
Dependent on customer requirements
|
Size Tolerance
|
Diameter Tolerance: ±0.1 mm
Length Tolerance: ±0.5 mm
|
Surface Finish
|
10/5, Refer to MIL-PRF-13830B Standard
|
Wavefront Distortion
|
λ/8 @ 633 nm
|
Flatness
|
λ/8 @ 633 nm
|
Parallelism
|
≤30"
|
Perpendicularity
|
≤15′
|
Chamfer
|
≤0.2 mm×45°
|
Extinction Ratio
|
≥25 dB
|
Reflectivity of Anti-reflection Coating
|
≤0.2% @ 2940 nm
|